Crack Formation in Concrete

Dr. Ulrike Rockland Pressestelle
Bundesanstalt für Materialforschung und -prüfung (BAM)

    Cracks in concrete structure elements can strongly prejudice their function and aesthetic appearance. Cracks cannot usually be avoided but their number and size can be controlled and it is technically feasible to close the cracks that form in many cases.

    Concrete is an artificial rock produced from cement, aggrgates (sand and gravel or broken stone) and water. It cannot be considered as a material with specified properties as these develop as a function of age and continue changing over time. Cement hardening and drying is usually accompanied by shrinkage, therefore fine cracks are inevitable. Cracks exceeding 0.1 mm can be handled by optimising the concrete composition and by using reinforcement.

    Crack formation caused by dynamic and static stress on concrete structure elements is due to working loads and permanent load. Thermal and chemical impacts and frost-deicing stress in the pore system of the concrete are also important. Suitably designed composition and/or preventive measures (hydrophobic treatment, coating) can long-lasting prevent weathering damages.

    Permanent weathering, horizontal surfaces, dark surfaces and sharp edges increase the risk of cracking formation and/or flaking due to increased thermal strain and unfavourable stresses in the building component. Avoiding cracks greater than 0.1 mm is often planned in the design phase for technical reasons (e.g. waterproof concrete). This may also be necessary on aesthetic causes.

    Before filling the cracks an appraisal has to be made to specify necessity, objectives and methods. Two techniques are applicable in principle to fill the cracks: soaking (filling the cracks without applying pressure) or injection (filling the cracks under pressure). Epoxy resins, polyurethane, cement paste or cement grouts are usually used for this purpose. The Guidelines of Concrete Repair of the German Committee for Reinforced Concrete of 2001 and/or DIN EN 1504 Part 5 and 9 regulate the relevant technical aspects.

    Contact:
    Dr.-Ing. Hans-Carsten Kühne
    Head of Working Group "Cementitious materials:
    advanced performance "
    Division VII.1 Building Materials
    Phone: +49 30 8104-3229
    Email: hans-carsten.kuehne@bam.de


    Images

    Criteria of this press release:
    Construction / architecture, Materials sciences
    transregional, national
    Research results, Transfer of Science or Research
    English


     

    Help

    Search / advanced search of the idw archives
    Combination of search terms

    You can combine search terms with and, or and/or not, e.g. Philo not logy.

    Brackets

    You can use brackets to separate combinations from each other, e.g. (Philo not logy) or (Psycho and logy).

    Phrases

    Coherent groups of words will be located as complete phrases if you put them into quotation marks, e.g. “Federal Republic of Germany”.

    Selection criteria

    You can also use the advanced search without entering search terms. It will then follow the criteria you have selected (e.g. country or subject area).

    If you have not selected any criteria in a given category, the entire category will be searched (e.g. all subject areas or all countries).